BMW Ireland Recall: Brake Servo Weld Defect Affects Multiple Models

On 07 January 2025, BMW Automotive (Ireland) Limited issued a voluntary recall affecting a wide range of BMW models, including the 2 Series, 5 Series, i5, 7 Series, i7, X1, iX1, X2, iX2, X5, X6, X7, XM, X5M, and X6M.

The recall addresses a manufacturing defect in the brake servomotor hollow shaft weld, which may lead to reduced braking performance and longer stopping distances, significantly increasing the risk of an accident.


Affected Vehicles

  • Models: BMW 2 Series, 5 Series, i5, 7 Series, i7, X1, iX1, X2, iX2, X5, X6, X7, XM, X5M, X6M
  • Market: Republic of Ireland
  • Production Dates: 06 July 2022 – 13 November 2024
  • Number of Vehicles Affected in Ireland: 4

Details of the Fault

The problem arises from a manufacturing defect in the servomotor’s hollow shaft weld. Specifically:

  • The weld may not withstand high braking pressure build-up.
  • If the weld breaks, braking performance is significantly reduced.
  • Drivers must apply greater force on the brake pedal.
  • Braking distance may increase, raising the risk of collisions.
  • Crucial systems such as ABS (Anti-lock Braking System) and DSC (Dynamic Stability Control) are not supported in this failure scenario.

Risks

  • Reduced braking performance – longer stopping distances.
  • Increased accident risk – particularly in emergency braking situations.
  • Safety systems compromised – ABS and DSC assistance unavailable.

What Owners Should Do

BMW advises all affected owners to:

  1. Check if their car is part of the recall (see steps below).
  2. Contact their nearest authorised BMW dealer immediately to arrange inspection and repair.
  3. Avoid delaying repairs, as this issue directly impacts vehicle braking safety.

Repairs will be carried out free of charge.


How to Check if Your Car is Affected

  • Visit the BMW Ireland recall check tool
  • Enter your Vehicle Identification Number (VIN)
  • Alternatively, contact BMW Customer Service or your local BMW dealership

Official Sources


FAQs

Q: Which BMW models are affected by this recall?
A: The recall covers the 2 Series, 5 Series, i5, 7 Series, i7, X1, iX1, X2, iX2, X5, X6, X7, XM, X5M, and X6M.

Q: How many vehicles are impacted in Ireland?
A: 4 vehicles are affected in the Republic of Ireland.

Q: What happens if the weld fails while braking?
A: Braking performance will be reduced, requiring greater pedal force, and the braking distance may increase, creating a higher risk of accident.

Q: Will I be charged for the repair?
A: No, BMW will cover all inspection and repair costs under this recall.


Disclaimer

This article is based on official recall information published by BMW Automotive (Ireland) Limited and the CCPC. It is intended for public safety awareness. Owners should verify details with BMW directly.

Leave a Reply

Your email address will not be published. Required fields are marked *